Silky Smooth Hydrating Makeup
ARL-20-79-1
Below are the cosmetic ingredients required for our Silky Smooth Hydrating Makeup for those who wish to make your own makeup or understand how our proprietary chemicals contribute to an excellent product.
| Phase | INGREDIENT | INCI | Supplier | % W/W |
|---|---|---|---|---|
| A | Deionized Water | 65.05 | ||
| A | Phoenoxol® BD-10P | PPG-10 Butanediol | Phoenix Chemical, Inc. | 2.50 |
| B | Glycerin 99.5% USP | Glycerin | Dow Chemical | 2.50 |
| B | Natrosol Plus 330 CS | Cetyl Hydroxyethylcellulose | Ashland | 0.10 |
| B | Keltrol T | Xanthan Gum | CP Kelco | 0.50 |
| C | SIH-5 TiO2 R250 | Titanium Dioxide (and) Silica (and) Aluminum Hydroxide | Kobo Products | 10.00 |
| C | SIH-2 YELLOW No.602P | Iron Oxides (CI 77492) (and) Silica | Kobo Products | 1.25 |
| C | SIH-2 RED No.211P | Iron Oxides (CI 77491) (and) Silica | Kobo Products | 0.75 |
| C | SIH-2 BLACK No.710P | Iron Oxides (CI 77499) (and) Silica | Kobo Products | 0.25 |
| C | Impact Matte Mica T | Mica | Sandream | 0.75 |
| C | Argel CBH White R.E.M | Bentonite | Arclay Natural | 0.75 |
| C | Softouch CC6059 Boron Nitride Powder | Boron Nitride | Momentive Performance Materials |
1.25 |
| D | Cerasynt SD | Glyceryl Stearate | Ashland | 0.50 |
| D | Pelemol® GMLA | Glyceryl Laurate | Phoenix Chemical, Inc. | 0.35 |
| D | Pelemol® D5R-V | Propanediol Dicaprylate/Caprate (and) Diisostearyl Malate | Phoenix Chemical, Inc. | 2.35 |
| D | Pelemol® P-810 | Propanediol Dicaprylate/Caprate | Phoenix Chemical, Inc. | 2.65 |
| D | Pelemol® P-1263 | Polyglyceryl-10 Hexaoleate (and) Polyglyceryl-6 Polyricinoleate | Phoenix Chemical, Inc. | 1.00 |
| D | Pelemol® DISM | Diisostearyl Malate | Phoenix Chemical, Inc. | 1.00 |
| D | Simulgreen 18-2 | Hydroxystearyl Alcohol (and) Hydroxystearyl Glucoside | Seppic Chemical | 1.50 |
| D | Pelemol® 899 | Isononyl Isononanoate (and) Ethylhexyl Isononanoate | Phoenix Chemical, Inc. | 5.00 |
| E | Preservative | q.s. | ||
| Total | 100.00 |
PROCEDURE:
- Combine Phase A with mixing and begin heating to 70°-75°C.
- Combine Phase B and add this blend to the water phase, mixing until gums have swelled.
- Premix and pulverize Phase C, then add Phase C to Phase A/B.
- Homogenize batch until Phase A/B/C is uniform.
- Maintain temeprature.
- In a separate vessel, combine Phase D and heat to 70°-75°C.
- When the temperature of the water phase (A/B/C) is the same as the temperature of the oil phase (D), add Phase D into Phase A/B/C under homogenization.
- Homogenize for 15 minutes or until batch is uniform throughout and all pigments are dispersed.
- Swtich to side sweep agitation. Begin to cool the batch to 45°-50°C. At 45°-50°C add Phase E and continue to mix using side sweep.
- Continue mixing and cooling the batch to room temperature.
| Ingredient | Function |
|---|---|
| Phoenoxol® BD-10P | Reduces heaviness and any greasiness in the formulation and adds light emolliency |
| Pelemol® GMLA | 100% vegetable derived emulsifier and conditioning agent |
| Pelemol® D5R-V | Cyclomethicone (D-5) replacement. Mimics all properties and aesthetics. 100% vegetable derived |
| Pelemol® P-810 | 100% vegetable derived dry ester. Helps reduce tack in finished formulation |
| Pelemol® P-1263 | Water-in-oil polymeric emulsifier |
| Pelemol® DISM | Adds light, silky emolliency |
| Pelemol® 899 | Light cushion ester. Reduces tack and improves spreadability |